Product Description of XHL-20 Film Creep Tester


The XHL-20 Film creep tester has a digital ruler system including a line laser pointer for manually measuring the creep.

The ruler is connected to the included computer via RS232 and the values are fed into a spreadsheet template which calculates the result.


Test Standards of XHL-20 Film Creep Tester

Product Features of XHL-20 Film Creep Tester

Parameter of Oven:

 

l The outer shell is made of cold-rolled steel plate, with surface electrostatic spraying, and the inner shell is made of mirror stainless steel. The partition can be adjusted freely;

 

l Adopting PMMA II operating system, the LCD screen displays various parameters, and the temperature control has functions such as temperature control, timing, and over temperature alarm;

 

l Adopting imported motors and blades, reasonable air ducts and circulation systems, to minimize temperature uniformity changes in the working room;

 

l 6-stage speed regulation of fan;

 

l The box door has a large viewing angle glass observation window, which is convenient for users to observe;

 

l Using nano material door seals and insulation materials to enhance performance;

l   Programmable programming, capable of setting 10 segments with 100 cycles;


Technical Parameter of XHL-20 Film Creep Tester

Temp. Range

RT+5-85℃

Temp. Resolution Ratio

0.1℃

Temp. Control Accuracy

±0.5℃

Temp. Uniformity

±2℃

Input Power

750W

Inner Chamber Size

600X520X750mm

Exterior Size

890X746X905mm

Timing Range

0-9999min/h

Load

1300g

Length Measurement Method

Laser

Length Measurement Range

0-300mm

Length Measurement Resolution

0.01mm

Illumination of the inner chamber

Built in

Dimension

890X746X905mm

Weight

150Kgs

Power Supply

220V, 50Hz, 1ph